Polymaker · PA

Fiberon PA612-CF

260–300°C
Nozzle temperature
Bed temperature
0.96
Flow ratio
orca filament flow ratio
8 mm³/s
Max volumetric speed
at 0.4 mm nozzle
Fan speed 10–30%
0%
100%

All settings

Nozzle temperature
260–300°C
Nozzle (first layer)
Bed temperature
Bed (first layer)
Flow ratio
0.96
Max volumetric speed
8 mm³/s (at 0.4 mm nozzle)
Fan speed
10–30%
Softening temperature
55°C (glass transition)

Sources: OrcaSlicer · material default (PA Tg ~55°C, Tm ~220°C)