Polymaker · PETG

Fiberon PET-CF

270–300°C
Nozzle temperature
Bed temperature
0.95
Flow ratio
orca filament flow ratio
12 mm³/s
Max volumetric speed
at 0.4 mm nozzle
Fan speed 0–?%
0%
100%

All settings

Nozzle temperature
270–300°C
Nozzle (first layer)
Bed temperature
Bed (first layer)
Flow ratio
0.95
Max volumetric speed
12 mm³/s (at 0.4 mm nozzle)
Fan speed
0–?%
Softening temperature
80°C (glass transition)

Sources: OrcaSlicer · Polymaker PolyLite PETG TDS