Snapmaker · PETG-CF

*Snapmaker PETG-CF @base*

245°C
Nozzle temperature
70°C
Bed temperature
First layer 70°C
0.95
Flow ratio
prusaslicer extrusion multiplier
Max volumetric speed
Fan speed 0–30%
0%
100%

All settings

Nozzle temperature
245°C
Nozzle (first layer)
250°C
Bed temperature
70°C
Bed (first layer)
70°C
Flow ratio
0.95
Max volumetric speed
Fan speed
0–30%
Softening temperature
82°C (glass transition)

Sources: PrusaSlicer · material default