Snapmaker · PETG

Dual PETG

255°C
Nozzle temperature
70°C
Bed temperature
First layer 70°C
0.95
Flow ratio
prusaslicer extrusion multiplier
Max volumetric speed
Fan speed 10–30%
0%
100%

All settings

Nozzle temperature
255°C
Nozzle (first layer)
255°C
Bed temperature
70°C
Bed (first layer)
70°C
Flow ratio
0.95
Max volumetric speed
Fan speed
10–30%
Softening temperature
80°C (glass transition)

Sources: PrusaSlicer · material default (ISO 11357 DSC)