Snapmaker · PETG

*Snapmaker Dual PET @base*

278°C
Nozzle temperature
65°C
Bed temperature
First layer 60°C
1
Flow ratio
prusaslicer extrusion multiplier
Max volumetric speed
Fan speed 26–50%
0%
100%

All settings

Nozzle temperature
278°C
Nozzle (first layer)
275°C
Bed temperature
65°C
Bed (first layer)
60°C
Flow ratio
1
Max volumetric speed
Fan speed
26–50%
Softening temperature
80°C (glass transition)

Sources: PrusaSlicer · material default (ISO 11357 DSC)