Snapmaker
·
PVA
Dual PVA @0.2 nozzle
220°C
Nozzle temperature
50°C
Bed temperature
First layer 50°C
1
Flow ratio
prusaslicer extrusion multiplier
—
Max volumetric speed
Fan speed
35–100%
0%
100%
All settings
- Nozzle temperature
- 220°C
- Nozzle (first layer)
- 220°C
- Bed temperature
- 50°C
- Bed (first layer)
- 50°C
- Flow ratio
- 1
- Max volumetric speed
- —
- Fan speed
- 35–100%
- Softening temperature
- 73°C (glass transition)
Sources: PrusaSlicer · material default