eSUN · PETG

PET Basic

280°C
Nozzle temperature
range 250–280°C
70°C
Bed temperature
Flow ratio
20 mm³/s
Max volumetric speed
at 0.4 mm nozzle
Nozzle range 280°C recommended
250°C
280°C
Fan speed 40–70%
0%
100%

All settings

Nozzle temperature
280°C (250–280)
Nozzle (first layer)
Bed temperature
70°C
Bed (first layer)
Flow ratio
Max volumetric speed
20 mm³/s (at 0.4 mm nozzle)
Fan speed
40–70%
Softening temperature
82°C (glass transition)

Sources: 3dfilamentprofiles.com · eSUN PETG TDS